Citation: Mm. Tagiev et al., HEAT-CONDUCTION OF EXTRUDED SAMPLES OF BI-SB SOLID-SOLUTIONS DOPED WITH TELLURIUM, Inorganic materials, 29(9), 1993, pp. 1076-1077
Citation: Mm. Tagiev et al., THERMAL-CONDUCTIVITY OF EXTRUDED SAMPLES OF LEAD-DOPED SOLID-SOLUTIONS OF THE BI-SB SYSTEM, Inorganic materials, 29(7), 1993, pp. 1082-1085
Citation: Mm. Tagiev et al., THERMOELECTRIC PROPERTIES OF EXTRUDED SPECIMENS OF BI0.85SB0.15 DOPEDWITH LEAD, Inorganic materials, 29(6), 1993, pp. 998-1000
Citation: Zf. Agaev et al., TEMPERATURE-DEPENDENCE OF THE ELECTRICAL CONDUCTIVITIES OF SOLID-SOLUTIONS OF THE BI2TE3-SB2TE3 AND BI2TE3-BI2SE3 SYSTEMS, Inorganic materials, 28(7), 1992, pp. 1259-1260