Authors: APPINO C FERRARA E FIORILLO F SUBERBIELLE I DEGAUQUE J LEBOURG C BARICCO M
Citation: C. Appino et al., ROLE OF SI CONCENTRATION ON THE MAGNETIC AND MECHANICAL-BEHAVIOR OF RAPIDLY SOLIDIFIED FE-SI LAMINATIONS, Journal de physique. IV, 8(P2), 1998, pp. 531-534

Authors: AUDISIO S IDRISSI H KHOMAMIZADEH F DEGAUQUE J APPINO C FERRARA E FIORILLO F ROCCHINO L SUBERBIELLE I BARICCO M
Citation: S. Audisio et al., MAGNETIC-PROPERTIES OF SILICON-IRON LAMINATIONS SI-ENRICHED BY A SIH4BASED CVD PROCESS, Journal de physique. IV, 8(P2), 1998, pp. 535-538

Authors: SHIN DW DEGAUQUE J ASTIE B
Citation: Dw. Shin et al., MAGNETOMECHANICAL BEHAVIOR IN GO AND NO FE-3-PERCENT-SI ALLOYS, Journal de physique. IV, 8(P2), 1998, pp. 539-542

Authors: BARICCO M MASTRANDREA E ANTONIONE C VIALA B DEGAUQUE J FERRARA E FIORILLO F
Citation: M. Baricco et al., GRAIN-GROWTH AND TEXTURE IN RAPIDLY SOLIDIFIED FE(SI) 6.5 WT-PERCENT RIBBONS, Materials science & engineering. A, Structural materials: properties, microstructure and processing, 226, 1997, pp. 1025-1029

Authors: FIORILLO F FERRARA E FERRANDO L APPINO C LEBOURG C DEGAUQUE J BARICCO M
Citation: F. Fiorillo et al., MAGNETIC LOSSES AND MECHANICAL-PROPERTIES OF FE-4 TO 7.8-WT-PERCENT-SI RAPIDLY QUENCHED ALLOYS, IEEE transactions on magnetics, 33(5), 1997, pp. 3802-3804

Authors: AUGUSTYNIAK B DEGAUQUE J
Citation: B. Augustyniak et J. Degauque, MICROSTRUCTURE INSPECTION BY MEANS OF MECHANICAL BARCHAUSEN EFFECT ANALYSIS, Journal de physique. IV, 6(C8), 1996, pp. 527-530

Authors: SHIN DW DEGAUQUE J LEBOURG C ASTIE B
Citation: Dw. Shin et al., INFLUENCE OF THERMAL-TREATMENT ON MAGNETOMECHANICAL DAMPING OF FE-49-CO-49-V-2 ALLOY, Journal de physique. IV, 6(C8), 1996, pp. 545-548

Authors: VIALA B DEGAUQUE J FAGOT M BARICCO M FERRARA E FIORILLO F
Citation: B. Viala et al., STUDY OF THE BRITTLE BEHAVIOR OF ANNEALED FE-6.5WT-PERCENT-SI RIBBONSPRODUCED BY PLANAR FLOW CASTING, Materials science & engineering. A, Structural materials: properties, microstructure and processing, 212(1), 1996, pp. 62-68

Authors: TANGUY A BRAS J DEGAUQUE J
Citation: A. Tanguy et al., DOMAIN-WALL PINNING IN NDFEB MELT-SPUN MAGNETS, Journal of magnetism and magnetic materials, 161, 1996, pp. 235-238

Authors: CROTTIERCOMBE S AUDISIO S DEGAUQUE J DELACHEISSERIE E PORTESEIL JL
Citation: S. Crottiercombe et al., SI-AL ENRICHED FE BASED SHEETS BY CHEMICAL-VAPOR-DEPOSITION - EVOLUTION OF MAGNETOELASTIC PROPERTIES, Journal of magnetism and magnetic materials, 161, 1996, pp. 292-298

Authors: CROTTIERCOMBE S AUDISIO S DEGAUQUE J PORTESEIL JL FERRARA E PASQUALE M FIORILLO F
Citation: S. Crottiercombe et al., THE MAGNETIC-PROPERTIES OF FE-SI 6.5WT-PERCENT ALLOYS OBTAINED BY A SICL4-BASED CVD PROCESS, Journal of magnetism and magnetic materials, 160, 1996, pp. 151-153

Authors: VIALA B DEGAUQUE J BARICCO M FERRARA E PASQUALE M FIORILLO F
Citation: B. Viala et al., MAGNETIC AND MECHANICAL-PROPERTIES OF RAPIDLY SOLIDIFIED FE-SI 6.5WT-PERCENT ALLOYS AND THEIR INTERPRETATION, Journal of magnetism and magnetic materials, 160, 1996, pp. 315-317

Authors: TANGUY A BINESTI D DEGAUQUE J BRAS J FAGOT M CHAMBEROD A
Citation: A. Tanguy et al., VANADIUM INFLUENCE IN NDFEBAL MELT-SPUN MAGNETS, Journal of magnetism and magnetic materials, 158, 1996, pp. 37-38

Authors: CROTTIERCOMBE S AUDISIO S DEGAUQUE J BERAUD C FIORILLO F BARICCO M PORTESEIL JL
Citation: S. Crottiercombe et al., EVOLUTION OF MAGNETOMECHANICAL AND MAGNETIC-PROPERTIES OF SILICONIZEDIRON-SILICON ALLOYS BY CVD PROCESS USING SICL4, Journal de physique. IV, 5(C5), 1995, pp. 1045-1052

Authors: AUGUSTYNIAK B DEGAUQUE J
Citation: B. Augustyniak et J. Degauque, NEW APPROACH TO HYSTERESIS PROCESS INVESTIGATION USING MECHANICAL ANDMAGNETIC BARKHAUSEN EFFECTS, Journal of magnetism and magnetic materials, 140, 1995, pp. 1837-1838

Authors: BILOTTE J FOURNIE G JOURET C SEGUELA A ASTIE B DEGAUQUE J FAGOT M
Citation: J. Bilotte et al., AN ORIGINAL DEVICE FOR OBSERVATIONS IN LORENTZ HVEM, Measurement science & technology, 5(4), 1994, pp. 394-399

Authors: CROTTIERCOMBE S DEGAUQUE J VIALA B BERAUD C ASTIE B AUDISIO S
Citation: S. Crottiercombe et al., EVOLUTION OF MAGNETOMECHANICAL DAMPING AND MAGNETIC-PROPERTIES OF PURE IRON SILICONIZED UP TO 5.5-WT-PERCENT BY CHEMICAL-VAPOR-DEPOSITION, Journal of alloys and compounds, 212, 1994, pp. 568-571

Authors: GANNAC Y DEGAUQUE J VIALA B REDOULES JP
Citation: Y. Gannac et al., MODELS OF THE MAGNETIC-BEHAVIOR OF GO AND NO (3.2 WT-PERCENT SI) AND RAPIDLY QUENCHED (6.5 WT-PERCENT SI) IRON SILICON ALLOYS, Journal of magnetism and magnetic materials, 133(1-3), 1994, pp. 63-66

Authors: ASTIE B FAGOT M BERAUD C DEGAUQUE J FERRARA E STANTERO A
Citation: B. Astie et al., OBSERVATIONS BY LORENTZ MICROSCOPY OF MOVEMENTS OF MAGNETIC DOMAIN-WALLS IN AMORPHOUS FE78B13SI9 ALLOYS, Journal of magnetism and magnetic materials, 133(1-3), 1994, pp. 77-81

Authors: CORTTIERCOMBE S AUDISIO S DEGAUQUE J VIALA B
Citation: S. Corttiercombe et al., SILICONIZATION AND ALUMINIZATION UP TO 6.5 WT-PERCENT OF IRON SHEETS - EVOLUTION OF MAGNETOMECHANICAL AND MAGNETIC-PROPERTIES, Journal of magnetism and magnetic materials, 133(1-3), 1994, pp. 205-208

Authors: FERRARA E FIORILLO F PASQUALE M STANTERO A BARICCO M DEGAUQUE J FAGOT M VIALA B DELACHEISSERIE ED PORTESEIL JL
Citation: E. Ferrara et al., ROLE OF MATERIAL PURITY ON THE STRUCTURAL AND MAGNETIC-PROPERTIES OF RAPIDLY SOLIDIFIED FESI 6.5 WT-PERCENT ALLOYS, Journal of magnetism and magnetic materials, 133(1-3), 1994, pp. 366-370

Authors: SNOECK E ROUCAU C BAULES P CASANOVE MJ FAGOT M ASTIE B DEGAUQUE J
Citation: E. Snoeck et al., USE OF IN-SITU TEM EXPERIMENTS FOR PHASE-TRANSITION STUDIES, Microscopy microanalysis microstructures, 4(2-3), 1993, pp. 249-264

Authors: DEGAUQUE J
Citation: J. Degauque, MAGNETISM AND MAGNETIC-MATERIALS - INTRODUCTION, Journal de physique. IV, 2(C3), 1992, pp. 1-13

Authors: GANNAC Y DEGAUQUE J REDOULES JP
Citation: Y. Gannac et al., MAGNETIC-PROPERTIES OF FE-6.5-PERCENT-SI ALLOYS PRODUCED BY RAPID SOLIDIFICATION IN CONTROLLED-ATMOSPHERE - COMPARISON WITH INDUSTRIAL FE-3.2-PERCENT-SI ALLOYS, Journal de physique. IV, 2(C3), 1992, pp. 79-83

Authors: BRAS J BIYADI K FAGOT M DEGAUQUE J
Citation: J. Bras et al., CRITICAL ENERGY OF SINGLE-DOMAIN ND2FE14B PARTICLES IN THIN MAGNETS, Journal de physique. IV, 2(C3), 1992, pp. 113-117