Citation: Mx. Guo et H. Suito, Dispersion of primary inclusions of Ce2O3 and CeS in Fe-0.20 mass%C-0.02 mass%P alloy, ISIJ INT, 39(7), 1999, pp. 678-686
Citation: Mx. Guo et H. Suito, Influence of dissolved cerium and primary inclusion particles of Ce2O3 andCeS on solidification behavior of Fe-0.20mass%C-0.02 mass%P alloy, ISIJ INT, 39(7), 1999, pp. 722-729
Citation: Mx. Guo et H. Suito, Pinning of austenite grain boundary of Fe-0.09 to 0.53 mass% C-0.02 mass%Palloys by primary inclusions of Ce2O3 and CeS, ISIJ INT, 39(12), 1999, pp. 1289-1296
Citation: Mx. Guo et H. Suito, Austenite grain size distribution and topological properties in Fe-0.09 to0.53 mass%C-0.02 mass%P alloys containing primary inclusions of Ce2O3 and CeS, ISIJ INT, 39(12), 1999, pp. 1297-1303
Citation: Mx. Guo et H. Suito, Effect of dissolved cerium on austenite grain growth in an Fe-0.20 mass%C-0.02 mass%P alloy, ISIJ INT, 39(11), 1999, pp. 1169-1175
Authors:
Morita, K
Mori, M
Guo, MX
Ikagawa, T
Sano, N
Citation: K. Morita et al., Activity of chromium oxide and phase relations for the CaO-SiO2-CrOX system at 1873 K under moderately reducing conditions, STEEL RES, 70(8-9), 1999, pp. 319-324