Authors: TU JP MENG L LIU MS
Citation: Jp. Tu et al., EVALUATION OF HYDROGEN EMBRITTLEMENT CHARACTERISTICS OF FE3AL INTERMETALLIC COMPOUNDS, Scripta materialia, 38(5), 1998, pp. 833-838

Authors: MENG L ZHENG XL TU JP LIU MS
Citation: L. Meng et al., EFFECTS OF DELETERIOUS IMPURITIES AND CERIUM MODIFICATION ON INTRINSIC AND EXTRINSIC TOUGHENING LEVELS OF AL-LI BASED ALLOYS, Materials science and technology, 14(6), 1998, pp. 585-591

Authors: TU JP MENG L LIU MS
Citation: Jp. Tu et al., FRICTION AND WEAR BEHAVIOR OF CU-FE3AL POWDER METALLURGICAL COMPOSITES IN DRY SLIDING, Wear, 220(1), 1998, pp. 72-79

Authors: TU JP LI ZZ MAO ZY
Citation: Jp. Tu et al., INTERNAL CHLORINATION OF NI BASED ALLOYS AND ITS RELATION TO VOLATILIZATION CORROSION, Werkstoffe und Korrosion, 48(7), 1997, pp. 441-446

Authors: TU JP LI J
Citation: Jp. Tu et J. Li, EFFECT OF PHASE-TRANSFORMATION INDUCED PLASTICITY ON THE EROSION OF TZP CERAMICS, Materials letters, 31(3-6), 1997, pp. 267-270

Authors: TU JP LIU MS
Citation: Jp. Tu et Ms. Liu, WET ABRASIVE WEAR OF ORDERED FE3AL ALLOYS, Wear, 209(1-2), 1997, pp. 31-36

Authors: TU JP LIU MS MAO ZY
Citation: Jp. Tu et al., EROSION RESISTANCE OF NI-WC SELF-FLUXING ALLOY COATING AT HIGH-TEMPERATURE, Wear, 209(1-2), 1997, pp. 43-48

Authors: TU JP
Citation: Jp. Tu, HIGH-TEMPERATURE CORROSION OF NICKEL-CHROMIUM ALLOYS IN FLOWING CHLORINE-WATER VAPOR ENVIRONMENTS, Corrosion, 53(5), 1997, pp. 365-373

Authors: TU JP LI ZZ MAO ZY
Citation: Jp. Tu et al., REACTION-MECHANISM OF PREOXIDIZED NICKEL-CHROMIUM-CERIUM ALLOY WITH CHLORINE GAS IN THE TEMPERATURE-RANGE 400-DEGREES-C TO 700-DEGREES-C, Corrosion, 53(4), 1997, pp. 312-318