Abstract
CVD-diamond films were deposited onto the titanium alloy Ti-6Al-4V. Sa mples were investigated in a ground and ultrasonically pretreated stag e and after different times of deposition. The coating time was varied between I and 210 min. SEM, XPS and Micro Raman spectroscopy were use d to characterize different stages of deposition. A model describing t he process of chemical vapor deposition of diamond onto Ti-6Al-4V is d eveloped. (C) 1997 Elsevier Science S.A.