Polystyrene-PEG crosslinked block copolymers were prepared from styren
e copolymerization by either poly(ethylene glycol dimethymethacrylate)
(PEG-DM) or macronomer initiators (MIM). M(w) values of PEG of PEG-DM
were 400, 600, 1000, 1500, 3000, 10,000, and 35,000, and of MIM, 400
and 1500. Swelling in H2O or CHCl3 of the sulfonated and unsulfonated
block copolymers were determined under comparable conditions and found
to be vary significantly. The ion-exchange capacity and selectivity c
oefficients of these ion-exchange resins were investigated. The capaci
ties of the obtained ion exchangers were varied between 0.4 and 2.9 me
q/g. (C) 1996 John Wiley & Sons, Inc.