PREPARATION TECHNOLOGY OF ELECTRONIC CERA MIC BATIO3 POWDER IN LIQUID-PHASE .2. STUDIES ON THE THERMAL-DECOMPOSITION REACTION-KINETICS OF PRECURSOR BATIO(C2O4)(2)CENTER-DOT-4H(2)O
D. Gu et al., PREPARATION TECHNOLOGY OF ELECTRONIC CERA MIC BATIO3 POWDER IN LIQUID-PHASE .2. STUDIES ON THE THERMAL-DECOMPOSITION REACTION-KINETICS OF PRECURSOR BATIO(C2O4)(2)CENTER-DOT-4H(2)O, Gaodeng xuexiao huaxue xuebao, 17(2), 1996, pp. 294-297
The kinetic parameters of the three steps of thermal decomposition of
the BaTiO(C2O4)(2) . 4H(2)O are calculated according to the Broido' s
linearized simple graphical procedure, It is shown that three-step-rea
ction orders are 2,2,0; the activation energies are 96.8, 165.1, 172.2
kJ/mol and that the frequency factors are 1.03 X 10(11), 5.64 X 10(8)
, 2.63 X 10(6) s(-1), respectively, The conditions of the process of t
hermal treatment are optimized according to the kinetic parameters. Th
e powder obtained are ultrafine BaTiO3 with a high purity.