Magnetization measurements to 2K and ac susceptibility measurements to
10mK have been performed on two intermediate valent SmB6 single cryst
als. The temperature dependence of susceptibility at temperatures abov
e 50K follows the van Vleck behaviour based on the contribution of 4f(
6) and 4f(5)5d(1) configurations of Sm - ions, and is in agreement wit
h the results obtained by other groups. Below 15K, however, the magnet
ization and susceptibility dependences seem to be strongly influenced
by impurities in the samples.