THERMOELECTROMOTIVE FORCE IN MAGNETIC AMORPHOUS-CRYSTALLINE FE79SI5B16 WIRE SYSTEMS

Citation
H. Chiriac et al., THERMOELECTROMOTIVE FORCE IN MAGNETIC AMORPHOUS-CRYSTALLINE FE79SI5B16 WIRE SYSTEMS, Journal of magnetism and magnetic materials, 160, 1996, pp. 239-240
Citations number
5
Categorie Soggetti
Material Science","Physics, Condensed Matter
ISSN journal
03048853
Volume
160
Year of publication
1996
Pages
239 - 240
Database
ISI
SICI code
0304-8853(1996)160:<239:TFIMAF>2.0.ZU;2-S
Abstract
The thermoelectromotive force supplied by the junction of an amorphous -crystalline wire thermocouple has been measured as a function of temp erature in the range 300-573 K. We have studied the effect of the addi tion of Cr to the Fe79Si5B16 alloy on the temperature dependence of th e thermoelectromotive force of the amorphous-crystalline thermocouples , The thermoelectromotive force is found to decrease with increasing a mounts of Cr.