Cm. Carr et al., THE EFFECT OF CORONA TREATMENTS ON THE HYGRAL EXPANSION OF WOOL WORSTED FABRICS, Journal of the Society of Dyers and Colourists, 110(12), 1994, pp. 383-386
The effect of dry corona and aqueous treatments on the hygral expansio
n of wool gabardine has been investigated. Increasing the severity of
the corona treatment produced a concomitant reduction in the hygral ex
pansion of the fabric. X-ray photoelectron spectroscopy has been used
to study the chemical modification of the wool fibre surface.