Surface acidity of aluminium oxide containing 5 wt.% lanthanum oxide h
as been determined by IR spectroscopy. Strength of Lewis sites of the
La2O3/Al2O3 system was lower than that of pure aluminium oxide, Howeve
r, the presence of La2O3 in aluminium oxide increased the thermostabil
ity of these sites in the mixed system.