Abstract
The rehealing ability of the protective oxide scales formed on a micro crystalline coating of the Ni-base superalloy K38G has been studied. T he results indicated that the oxide scales on the coating may be rehea led when the original scales ale destroyed and the coating still has e xcellent resistance against high-temperature oxidation. When the origi nal Al2O3 oxide scales spall, mixed-oxide scales of both (Al, Cr)(2)O- 3 and TiO2 can form on the surface. The mixed scales are very protecti ve and adherent.