A. Dechirico et al., DIFFERENTIAL SCANNING CALORIMETRY AND THERMAL GRAVIMETRIC ANALYSIS OFLIGNIN BLENDED WITH TRIGLYCIDYL ISOCYANURATE, Die Angewandte makromolekulare Chemie, 228, 1995, pp. 51-58
The thermal behaviour of lignin blended with triglycidyl isocyanurate
(TGI) was investigated by differential scanning calorimetry (DSC) and
thermogravimetric analysis (TG) over a range of lignin contents from 0
to 85 wt.-%. DSC thermograms of lignin/TGI blends show two exothermic
peaks at about 250 and 355 degrees C while TG analysis in nitrogen be
ars evidence of a single loss of weight at about 360 degrees C. The fi
rst exotherm is suggested to correspond to the heat of bulk reaction b
etween epoxy groups of TGI with phenolic hydroxy groups of lignin, and
the second one to the heat of char formation of lignin. TG and infrar
ed analyses suport this conclusion.