A. Aruga et al., SYNTHESIS OF 0.4PB(MG1 3NB2/3)O3-0.3PB(MG1/2W1/2)O3-0.3PBTIO3 CERAMICS BY METAL ALKOXIDE METHOD, AND ITS DIELECTRIC-PROPERTIES/, Journal of the American Ceramic Society, 76(11), 1993, pp. 2939-2941
0.4Pb(Mg1/3Nb2/3)O3-0.3Pb(Mg1/2W1/2)O3-0.3PbTiO3 + xMgO (x = 0 to 0.04
) were prepared by a metal alkoxide method. The percent of perovskite
phase of the calcined powders increased with increased calcination tem
peratures. About 89% of perovskite phase was obtained at 1050-degrees-
C. The dielectric constant of the pellets fired at 1100-degrees-C was
increased by the addition of 10 wt% excess Mg(OC2H5)2 and had a maximu
m value of 7532 at 1 kHz.