Magnetic relaxation measurements were performed in the temperature ran
ge 200<T(K)<800 on vacancy-doped polycrystalline magnetite. Important
relaxation peaks have been observed in the temperature ranges 250<T(K)
<350 (peak III) and 400<T(K)<600 (peak I). Particular attention has be
en focused on the behavior of peak I where isothermal measurements hav
e extended over times up to 10(5) s. It is argued that the main featur
es of peak I are compatible with a dislocation relaxation.