ACTIVATION PARAMETERS OF THE ZENER PEAK IN CU-LI ALLOYS PRODUCED BY ELECTRODEPOSITION

Citation
Oa. Lambri et al., ACTIVATION PARAMETERS OF THE ZENER PEAK IN CU-LI ALLOYS PRODUCED BY ELECTRODEPOSITION, Journal de physique. IV, 6(C8), 1996, pp. 89-92
Citations number
10
Categorie Soggetti
Physics
Journal title
ISSN journal
11554339
Volume
6
Issue
C8
Year of publication
1996
Pages
89 - 92
Database
ISI
SICI code
1155-4339(1996)6:C8<89:APOTZP>2.0.ZU;2-G
Abstract
Copper-lithium alloys were produced by electrodeposition. They show a Zener peak at 650 K (at 0.2 s(-1)) which appears overlapped with the l ow and intermediate temperature grain boundary damping peaks of copper and also with the phase transition peak related to Cu-18 at% Li cryst als. In this work the activation energy, H, and the pre-exponential fa ctor tau(0) were calculated. Those were H = (160 +/- 4) KJ/mol and tau (0) = 2 x 10((-14 +/- 1)) (s).