Workplace air measurements are presented for PBDDs and PBDFs. These me
asurements were taken during extruder production and injection molding
of a PBTP-polymer blended with glass fiber, Sb2O3, and tetrabromobisp
henol A carbonate oligomer powder or PBTP-BC52-batch. The extruder gra
nulate and the molded test articles were also analyzed. The sampling t
rains, technique and plans, as well as the preparation, clean up and d
etermination methods were further developed on the basis of our previo
us work in this field1,5. No 2,3,7,8-isomer-substituted PBDDs and PBDF
s could be detected. The values monitored for the other isomers (tetra
- to hexabromo-compounds) were in the region of 30 to 260 pg/m3.