K. Saegusa et al., EFFECT OF COMPOSITION AND SIZE OF CRYSTALLITE ON CRYSTAL PHASE IN LEAD BARIUM-TITANATE, Journal of the American Ceramic Society, 76(6), 1993, pp. 1505-1512
Lead titanate, barium titanate, and lead barium titanate powders (>99.
9% pure), the particle size of which varied from 0.03 to 0.15 mum depe
nding on the calcination temperature and the composition, was-prepared
from barium lead titanyl oxalate, which was previously prepared by re
acting high-purity ammonium titanyl oxalate with barium and lead aceta
te. The critical crystallite size of BaTiO3 powder from the cubic to t
he tetragonal phase is around 1 mum. Pb0.3Ba0.7TiO3 powder with an ave
rage size of 0.057 mum showed the tetragonal phase.