ORIENTATION AND TEMPERATURE-DEPENDENCE OF WORK-HARDENING RATE IN CD SINGLE-CRYSTALS

Authors
Citation
N. Ucar, ORIENTATION AND TEMPERATURE-DEPENDENCE OF WORK-HARDENING RATE IN CD SINGLE-CRYSTALS, Physica status solidi. a, Applied research, 160(1), 1997, pp. 29-33
Citations number
26
Categorie Soggetti
Physics, Condensed Matter
ISSN journal
00318965
Volume
160
Issue
1
Year of publication
1997
Pages
29 - 33
Database
ISI
SICI code
0031-8965(1997)160:1<29:OATOWR>2.0.ZU;2-G
Abstract
The orientation and temperature dependence of the work hardening rate (WHR) has been investigated in tension in the temperature range from r oom temperature to 500 K in Cd single crystals. The WHR was found to d ecrease rapidly with increasing temperature. For [2<$(11)over bar $>3] orientated crystals, the WHR increases firstly with increasing temper ature until it passes a maximum at about 350 K.