Carbon fiber-reinforced (YMAS) glass-ceramic matrix composites. III. Interfacial aspects

Citation
V. Bianchi et al., Carbon fiber-reinforced (YMAS) glass-ceramic matrix composites. III. Interfacial aspects, J EUR CERAM, 19(3), 1999, pp. 317-327
Citations number
35
Categorie Soggetti
Apllied Physucs/Condensed Matter/Materiales Science","Material Science & Engineering
Journal title
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY
ISSN journal
09552219 → ACNP
Volume
19
Issue
3
Year of publication
1999
Pages
317 - 327
Database
ISI
SICI code
0955-2219(1999)19:3<317:CF(GMC>2.0.ZU;2-3
Abstract
Unidirectional continuous carbon fiber-reinforced glass-ceramic matrix comp osites have been fabricated for dry sliding applications. Different fractur e behaviors have been observed (three-point bend test and fracture surfaces observation). Besides, the distance between next microcracks, which have a ppeared in the matrix on cooling after hot-pressing of the composites, chan ges with the sintering temperature, suggesting fiber-matrix reactions. The nature of the fiber-matrix interface is observed in Transmission Electronic Microscopy and the interfacial shear stress is determined by push-in tests . (C) 1998 Elsevier Science Limited. All rights reserved.