Layered titanium phosphates and heat-treated tin phosphate showed high
separation factors (1.015-1.018) for lithium isotopes; the fractionat
ion properties could be explained by considering two factors: the degr
ee of Li+ dehydration in the solid phase and the affinity of the ion-e
xchange site toward Li+.