Hydrogen interaction with Ce2N0.8Si1.2, Ce2NiSi, Ce2Ni1.2Si0.8 and Ce6Ni2Si
3 compounds were studied. The new hydride phases containing 3.7, 4.4, 4.9,
and 10.9 hydrogen atoms per formula unit correspondingly, have been synthes
ized and characterized by X-ray diffraction and thermodesorption methods. A
ll hydrides preserved structure type of the starting compounds with pronoun
ced anisotropic distortion of crystal lattice. Some suggestions on hydrogen
localization in interstitial sites have been proposed. (C) 1999 Internatio
nal Association for Hydrogen Energy. Published by Elsevier Science Ltd. All
rights reserved.