A novel anti-condensation ship coating is discussed, and equipment des
igned for evaluating the performance of the coating quantitatively is
described. An isobutylene-anhydride based copolymer was synthesized an
d used as a water-absorbing resin instead of a starch-based water-abso
rbing resin currently used in the coatings. Expanded perlite was used
as the heal insulation material. The optimum formulation was determine
d to be titanium dioxide powder 5.1 g (8.26%); perlite 12 g (19.44%);
zeolite 13 g (21.06%); water-absorbing resin 3 g (4.86%); tributyl-pho
sphate 0.3 g (0.49%); emulsifier OP-10 0.3 g (0.49%); and styrene-acry
late copolymer emulsion 28 g (45.38%).