A homogeneous composite of poly(thiophenylenesulfonic acid) (1)/poly(oxyeth
ylene) (2) was prepared. The composite has a glass transition temperature a
t 5.0 degrees C and shows a proton conductivity of 1.2 x 10(-5) S cm(-1) at
30 degrees C under nonaqueous conditions. The conductivity increases with
the temperature up to about 10(-3) S cm(-1). The composite film keeps the s
ame conductivity value after treatment at 130 degrees C for 100 h.