The influence of Sr on the crystal structure, microstructure, and thermal e
xpansion of Ba0.98Sr0.02Ti1-xMnxO3 ceramics (0 less than or equal to x less
than or equal to 0.02) was investigated. Compared to Sr-"free" samples the
: transition region between tetragonal and hexagonal phase is shifted to si
gnificant higher Mn concentrations. Mn contents higher than 2.0 mol% strong
ly hinder grain growth at 1400 degrees C. The Goldschmidt tolerance factor
is used to discuss the stabilization of the tetragonal phase by the Sr impu
rity. (C) 2000 Elsevier Science B.V. Ail rights reserved.