Reduction of celestite (SrSO4) powder with particles of active charcoal has
been studied extensively in the absence and presence of catalysts. The opt
imum temperature at the charging zone has been optimized to get a maximum w
ater-soluble strontium sulfide value. The strontium value has been analyzed
using a chemical method, which was verified by the instrumental method usi
ng an inductively coupled plasma-optical emission spectrophotometer (ICP-OE
S). The conversion-time data have been analyzed by using a modified volume-
reaction (MVR) model, and the effect of the catalyst on kinetic parameters
has been elucidated. It was found that potassium carbonate, potassium dichr
omate, sodium carbonate, and sodium dichromate catalysts were found to enha
nce the reaction rate quite satisfactorily in the reduction of the celestit
e (SrSO4).