Thermal degradation studies of some aliphatic polyamides using hyphenated techniques (TG-MS, TG-FTIR)

Citation
M. Herrera et al., Thermal degradation studies of some aliphatic polyamides using hyphenated techniques (TG-MS, TG-FTIR), J THERM ANA, 59(1-2), 2000, pp. 385-394
Citations number
14
Categorie Soggetti
Spectroscopy /Instrumentation/Analytical Sciences
Journal title
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY
ISSN journal
13886150 → ACNP
Volume
59
Issue
1-2
Year of publication
2000
Pages
385 - 394
Database
ISI
SICI code
1388-6150(2000)59:1-2<385:TDSOSA>2.0.ZU;2-0
Abstract
The thermal degradation of the aliphatic polyamides 6 and 66 was investigat ed by means of the combined techniques TA-MS and TA-FTIR. The analyses were performed in three different devices. Sample mass ranged from 13 mg to 1 g and heating rates of 2.6 and 10 K min(-1) were used in both air and nitrog en atmospheres. The most important decomposition products were caprolactam for PA 6 and cyclopentanone for PA 66. Evolution of NH3 and HCN was registe red. The findings of the two hyphenated techniques led to the same results and complemented each other well. The evolved products were captured and an alyzed off-line by GC/MS for further confirmation of results.