A strain-gauge procedure that enables determination of the crack-tip toughn
ess (K-I0) from bending-strength tests is described, The procedure is appli
ed to coarse-grained alumina: and yields an average K-I0 value of 2.51 MPa.
m(1/2) with a standard deviation of 0.16 MPa.m(1/2).