Mechanical activation during grinding affects the flotability of pyrite, ar
senopyrite, and galena. It is established that the S, Fe, and As atoms at t
he surfaces of the initial materials are mainly in the oxidized state. The
transformations occurring on the surfaces of mechanically activated sulfide
minerals are the cause of the changes in flotability.