Ti-Al-Cu series burn-resistant alloys are newly developed materials which h
ave low density, low cost and are easy to process. The results show that Ti
-Al-Cu alloys have good burn resistance due to their good thermal conductiv
ity, low melting point, and the existence of Ti2Cu phase which also has a v
ery low melting point. Ti-Al-Cu alloys have excellent thermal processabilit
y and good room and high temperature tensile properties, but an increase in
copper content harms their thermal stability. After thermal exposure for a
long time, Ti2Cu phase will coalesce and coarsen, but the addition of Si a
nd Al will be useful for their thermal stability. The Ti-13Cu-1Al-0.2Si all
oy has good thermal stability at 540 degreesC and good creep resistance at
300 degreesC and 100 MPa. The phases of Ti-Al-Cu alloys were found to be co
mposed of alpha phase and Ti2Cu. The character of the Ti2Cu phase changes w
ith the increasing copper content.