A plastic optical fibre (POF) transmission experiment utilising green LEDs at a wavelength of 520nm is reported. The transmission loss of the 100m POF was 10dB, which is considerably lower than the loss for red (660nm) and bl ue (470nm) LEDs. The receiver sensitivity at 30Mbit/s was -20.8dB at 10(-9) bit error rate, which suggests the possibility of a longer length signal t ransmission, 200m or longer.