A homologous series of ring-substituted dialkoxy-PPV precursors have b
een synthesized and characterized. By increasing the number of methyle
ne units in the side groups up to six, a linear decrease of the glass
transition temperature is found, with a span of ca. 100 degrees C, goi
ng from 92 degrees C down to -11 degrees C. T.m.a. experiments reveal
high stretchability of thin films at temperatures just above T-g witho
ut elimination. The thermal conversion of the precursor polymer into t
he conjugated materials was studied and with controllable amounts of c
atalytic acid in the thin films, a well-defined processing window can
be established in order to prepare stretched, conjugated thin films of
dialkoxy-PPV material. Copyright (C) 1996 Elsevier Science Ltd.