Poly(trimethylene terephthalate) (PTT) has been polymerized at temperatures
between 150 and 220 degreesC as extended chain lamellar single crystals, c
a 100 Angstrom thick, by the confined thin film melt polymerization (CTFMP)
technique. The crystal structure, determined from electron diffraction pat
terns and modeling using the CERIUS2 simulation program is compared with th
at of solution gown crystals from higher molecular weight commercial PTT an
d PTT polymerized in the hulk at temperatures from 180 to 220 degreesC; the
crystal density is highest for the CTFMP material and least for the soluti
on precipitated commercial PTT. The triclinic unit cell of PTT contains two
chemical repeat units from a single chain, with lattice parameters of a =
4.53, b = 6.15, c = 18.61 Angstrom, alpha = 97 degrees, beta = 92 degrees,
gamma = 111 degrees, rho = 1.448 g/cm(3). (C) 2001 Elsevier Science Ltd. Al
l rights reserved.