Elastomeric polyaniline was prepared by being mixed with ethylene-propylene
-diene (EPDM) rubber in low concentrations (10, 20, or 30 wt %). The mixtur
e was made in an internal mixer coupled to a torque rheometer. The polyanil
ine was doped with dodecylbenzenesulfonic acid (DBSA) via reactive processi
ng during the mixing. When the EPDM rubber was added to the polyaniline and
DBSA, the doping reaction was not interrupted, as demonstrated by an incre
ase in the torque values. We chose the relative DBSA and EPDM concentration
s to obtain the highest conductivities (10(-1) to 10(-3) S cm(-1)) and the
best mechanical properties. (C) 2001 John Wiley & Sons, Inc.