Assessment of shear bond strength between three denture reline materials and a denture base acrylic resin
Citation
Y. Takahashi et J. Chai, Assessment of shear bond strength between three denture reline materials and a denture base acrylic resin, INT J PROST, 14(6), 2001, pp. 531-535
Categorie Soggetti
Dentistry/Oral Surgery & Medicine
Journal title
INTERNATIONAL JOURNAL OF PROSTHODONTICS
SICI code
0893-2174(200111/12)14:6<531:AOSBSB>2.0.ZU;2-F
Abstract
Purpose: This study reports the effect of five surface treatments on the bo
nd strength established between three denture reline materials and a dentur
e base resin. Materials and Methods: Cylindric columns of denture reline ma
terials were bonded to columns of denture base resins that received one of
the surface treatments: application of dichloromethane, the monomer of the
denture base resin, the recommended bonding agent or the monomer of the den
ture reline material, polishing with 240-grit silicone carbide paper, and a
ir abrasion. A control group without surface treatment was included for eac
h material. Specimens were immersed in water for 1 day and then thermocycle
d. The strength at which the bond failed under shear was recorded. Results:
None of the surface treatments significantly improved the bond strength of
Kooliner. Triad bonding agent and denture base monomer applications most s
ignificantly improved the bond strengths of Triad and GC reline, respective
ly. Conclusion: Triad bonding agent and denture base monomer should be used
in conjunction with Triad and GC reline, respectively, when relining a den
ture base resin.