In the series of articles [1,2,3] the possibilities assessment of changes i
n the thickness of non-woven under the effect of cyclic dynamic loads have
been presented. In this publication an original measuring stand and the res
ults of comparative tests for certified non-woven samples, indicating the p
resence of significant differences in the lateral deformation compared to t
raditional investigation methods, are presented.