Authors: Kohopaa, J Ahlstrand, R
Citation: J. Kohopaa et R. Ahlstrand, Re-embrittlement behaviour of VVER-440 reactor pressure vessel weld material after annealing, INT J PRES, 77(10), 2000, pp. 575-584

Authors: Shtrombakh, YI
Citation: Yi. Shtrombakh, Examination of VVER-440 RPV steel re-irradiation behavior using materials from operating units, INT J PRES, 77(10), 2000, pp. 585-590

Authors: Rosinski, ST Server, WL
Citation: St. Rosinski et Wl. Server, Application of the Master Curve in the ASME code, INT J PRES, 77(10), 2000, pp. 591-598

Authors: Lee, BS Hong, JH Yang, WJ Huh, MY Chi, SH
Citation: Bs. Lee et al., Master Curve characterization of the fracture toughness in unirradiated and irradiated RPV steels using full- and 1/3-size pre-cracked Charpy specimens, INT J PRES, 77(10), 2000, pp. 599-604

Authors: Serrano, M Perosanz, FJ Lapena, J
Citation: M. Serrano et al., Direct measurement of reactor pressure vessel steels fracture toughness: Master Curve concept and instrumented Charpy-V test, INT J PRES, 77(10), 2000, pp. 605-612

Authors: Langer, R Backfisch, W Bartsch, R
Citation: R. Langer et al., Results and evaluations of irradiation surveillance programmes of lightwater reactors in Germany, INT J PRES, 77(10), 2000, pp. 613-620

Authors: Priest, RH Belcher, WPA Mendes, CM Neale, BK
Citation: Rh. Priest et al., Irradiation surveillance data for an A508 forging and associated weld metal, INT J PRES, 77(10), 2000, pp. 621-628

Authors: Bischler, PJE Callen, VM Corcoran, RC Spellward, P
Citation: Pje. Bischler et al., A microstructural examination of irradiated reactor pressure vessel weld samples, INT J PRES, 77(10), 2000, pp. 629-640

Authors: Davies, M
Citation: M. Davies, Special issue - Irradiation embrittlement of Reactor Pressure Vessel steels, INT J PRES, 77(10), 2000, pp. III-IV

Authors: Ainsworth, RA
Citation: Ra. Ainsworth, Untitled, INT J PRES, 77(1), 2000, pp. 1-1

Authors: Rahman, S Chen, G Firmature, R
Citation: S. Rahman et al., Probabilistic analysis of off-center cracks in cylindrical structures, INT J PRES, 77(1), 2000, pp. 3-16

Authors: Chen, HF Shu, DW
Citation: Hf. Chen et Dw. Shu, Lower and upper bound limit analyses for pipeline with multi-slots of various configurations, INT J PRES, 77(1), 2000, pp. 17-25

Authors: Sim, CM Chang, KO Sohn, JM Chon, BS Baik, HK
Citation: Cm. Sim et al., Burg spectrum estimation of neutron noise for the monitoring of reactor internal vibration with a hypothesis test, INT J PRES, 77(1), 2000, pp. 27-33

Authors: Vilhelmsen, T
Citation: T. Vilhelmsen, Reference stress solutions of flat end to cylindrical shell connection andcomparison with design stresses predicted by codes, INT J PRES, 77(1), 2000, pp. 35-39

Authors: Timofeev, BT Karzov, GP Blumin, AA Anikovsky, VV
Citation: Bt. Timofeev et al., Fracture toughness of 15X2MFA steel and its weldments, INT J PRES, 77(1), 2000, pp. 41-52

Authors: Mackerle, J
Citation: J. Mackerle, Creep and creep fracture/damage finite element modelling of engineering materials and structures - A bibliography (1980-1999), INT J PRES, 77(1), 2000, pp. 53-77

Authors: Redekop, D Xu, B Zhang, YM
Citation: D. Redekop et al., Stability of a toroidal fluid-containing shell, INT J PRES, 76(9), 1999, pp. 575-581

Authors: Zhang, X
Citation: X. Zhang, A study on crack growth in ductile materials, INT J PRES, 76(9), 1999, pp. 583-590

Authors: Holzmann, M Dlouhy, I Brumovsky, M
Citation: M. Holzmann et al., Measurement of fracture toughness transition behaviour of Cr-Ni-Mo-V pressure vessel steel using pre-cracked Charpy specimens, INT J PRES, 76(9), 1999, pp. 591-598

Authors: Perrin, IJ Hayhurst, DR
Citation: Ij. Perrin et Dr. Hayhurst, Continuum damage mechanics analyses of type IV creep failure in ferritic steel crossweld specimens, INT J PRES, 76(9), 1999, pp. 599-617

Authors: Chen, J Shi, Y Shi, S
Citation: J. Chen et al., Noise analysis of digital ultrasonic nondestructive evaluation system, INT J PRES, 76(9), 1999, pp. 619-630

Authors: Kim, YW Kim, JI Chang, MH
Citation: Yw. Kim et al., An explicit integral expression for the stress intensity factor of a semi-elliptic surface crack subjected to thermal transient loading, INT J PRES, 76(9), 1999, pp. 631-639

Authors: Xing, J Hong, YJ
Citation: J. Xing et Yj. Hong, A maximum likelihood method for estimates of the statistics of the crack growth behavior, INT J PRES, 76(9), 1999, pp. 641-646

Authors: Han, LH Deng, YC Liu, CD
Citation: Lh. Han et al., The determination of J(IC) for polyethylene pipe using non-standard arc-shaped specimen, INT J PRES, 76(9), 1999, pp. 647-651

Authors: Wang, WQ Liu, CJ Zhou, SJ
Citation: Wq. Wang et al., On the probabilistic failure assessment diagram, INT J PRES, 76(9), 1999, pp. 653-662
Risultati: << | 101-125 | 126-150 | 151-175 | 176-200 | >>