Citation: Ra. De Souza et al., A SIMS study of oxygen tracer diffusion and surface exchange in La0.8Sr0.2MnO3+delta, MATER LETT, 43(1-2), 2000, pp. 43-52
Citation: Ja. Lane et Ja. Kilner, Measuring oxygen diffusion and oxygen surface exchange by conductivity relaxation, SOL ST ION, 136, 2000, pp. 997-1001
Citation: Ckm. Shaw et al., Mixed cobalt and nickel containing perovskite oxide for intermediate temperature electrochemical applications, SOL ST ION, 135(1-4), 2000, pp. 765-769
Citation: D. Waller et al., The effect of pulse duration and oxygen partial pressure on La0.7Sr0.3CoO3-delta and La0.7Sr0.3Co0.2Fe0.8O3-delta films prepared by laser ablation, SOL ST ION, 134(1-2), 2000, pp. 119-125
Citation: Ra. De Souza et Ja. Kilner, Oxygen transport in La1-xSrxMn1-yCoyO3 +/-delta perovskites part II. Oxygen surface exchange, SOL ST ION, 126(1-2), 1999, pp. 153-161
Citation: V. Dusastre et Ja. Kilner, Optimisation of composite cathodes for intermediate temperature SOFC applications, SOL ST ION, 126(1-2), 1999, pp. 163-174
Citation: Sj. Benson et al., Degradation of La0.6Sr0.4Fe0.8Co0.2O3-delta in carbon dioxide and water atmospheres, J ELCHEM SO, 146(4), 1999, pp. 1305-1309
Authors:
Ruiz-Trejo, E
Sirman, JD
Baikov, YM
Kilner, JA
Citation: E. Ruiz-trejo et al., Oxygen ion diffusivity, surface exchange and ionic conductivity in single crystal Gadolinia doped Ceria, SOL ST ION, 115, 1998, pp. 565-569