Citation: Av. Simakin et al., Self-limiting of the thickness of diamond-like films deposited in the laser pyrolysis of liquid aromatic hydrocarbons, QUANTUM EL, 30(3), 2000, pp. 263-267
Citation: Aa. Edigaryan et al., Kinetics of the codischarge of nickel and chromium ions from oxalate-sulfate solutions into an alloy, PROT MET R, 36(6), 2000, pp. 515-519
Citation: En. Lubnin et al., X-ray photoelectron spectroscopy of chromium layers electroplated from oxalate-sulfate solutions, PROT MET R, 36(4), 2000, pp. 301-305
Authors:
Tsar'kova, OG
Garnov, SV
Konov, VI
Lubnin, EN
Obraztsova, ED
Dausinger, F