Authors: Willems, G Clocheret, K Celis, JP Verbeke, G Chatzicharalampous, E Carels, C
Citation: G. Willems et al., Frictional behavior of stainless steel bracket-wire combinations subjectedto small oscillating displacements, AM J ORTHOD, 120(4), 2001, pp. 371-377

Authors: Zhang, XL Lauwerens, W Stals, L He, JW Celis, JP
Citation: Xl. Zhang et al., Fretting wear rate of sulphur deficient MoSx coatings based on dissipated energy, J MATER RES, 16(12), 2001, pp. 3567-3574

Authors: Gunzel, R Shevshenko, N Matz, W Mucklich, A Celis, JP
Citation: R. Gunzel et al., Structural investigation and wear resistance of submicron TiN coatings obtained by a hybrid plasma immersion ion implantation process, SURF COAT, 142, 2001, pp. 978-983

Authors: de Wit, E Drees, D Wu, PO Celis, JP
Citation: E. De Wit et al., Lubricating reaction products on TiN coatings during slic wear in phosphoric acid (vol 135, pg 8, 2000), SURF COAT, 140(3), 2001, pp. 302-302

Authors: Wang, JH Lauwerens, W Wieers, E Stals, LM He, JW Celis, JP
Citation: Jh. Wang et al., Structure and tribological properties of MoSx coatings prepared by bipolarDC magnetron sputtering, SURF COAT, 139(2-3), 2001, pp. 143-152

Authors: Garcia, I Drees, D Celis, JP
Citation: I. Garcia et al., Corrosion-wear of passivating materials in sliding contacts based on a concept of active wear track area, WEAR, 249(5-6), 2001, pp. 452-460

Authors: Zhang, X Vitchev, RG Lauwerens, W Stals, L He, J Celis, JP
Citation: X. Zhang et al., Effect of crystallographic orientation on fretting wear behaviour of MoSx coatings in dry and humid air, THIN SOL FI, 396(1-2), 2001, pp. 69-77

Authors: Cerisier, M Attenborough, K Jedryka, E Wojcik, M Nadolski, S Van Haesendonck, C Celis, JP
Citation: M. Cerisier et al., Structural study of nanometric electrodeposited Co films using Co-59 NMR, J APPL PHYS, 89(11), 2001, pp. 7083-7085

Authors: Hirato, T Fransaer, J Celis, JP
Citation: T. Hirato et al., Electrolytic codeposition of silica particles with aluminum from AlCl3-dimethylsulfone electrolytes, J ELCHEM SO, 148(4), 2001, pp. C280-C283

Authors: Dedeloudis, C Fransaer, J Celis, JP
Citation: C. Dedeloudis et al., Surface force measurements at a copper electrode/electrolyte interface, J PHYS CH B, 104(9), 2000, pp. 2060-2066

Authors: Basu, B Vitchev, RG Vleugels, J Celis, JP van der Biest, O
Citation: B. Basu et al., Influence of humidity on the fretting wear of self-mated tetragonal zirconia ceramics, ACT MATER, 48(10), 2000, pp. 2461-2471

Authors: Ruythooren, W Attenborough, K Beerten, S Merken, P Fransaer, J Beyne, E Van Hoof, C De Boeck, J Celis, JP
Citation: W. Ruythooren et al., Electrodeposition for the synthesis of microsystems, J MICROM M, 10(2), 2000, pp. 101-107

Authors: Attenborough, K Boeve, H de Boeck, J Borghs, G Celis, JP
Citation: K. Attenborough et al., Ultra-sensitive spin-valve structures grown on n-GaAs by single bath electrodeposition, SENS ACTU-A, 81(1-3), 2000, pp. 9-12

Authors: Huq, MZ Butaye, C Celis, JP
Citation: Mz. Huq et al., An innovative system for fretting wear testing under oscillating normal force, J MATER RES, 15(7), 2000, pp. 1591-1599

Authors: de Wit, E Drees, D Wu, PQ Celis, JP
Citation: E. De Wit et al., Lubricating reaction products on TiN coatings during sliding wear in phosphoric acid, SURF COAT, 135(1), 2000, pp. 8-13

Authors: Lauwerens, W Wang, JH Navratil, J Wieers, E D'haen, J Stals, LM Celis, JP Bruynseraede, Y
Citation: W. Lauwerens et al., Humidity resistant MoSx films prepared by pulsed magnetron sputtering, SURF COAT, 131(1-3), 2000, pp. 216-221

Authors: Wu, PQ Chen, H Van Stappen, M Stals, L Celis, JP
Citation: Pq. Wu et al., Comparison of fretting wear of uncoated and PVD TiN coated high-speed steel under different testing conditions, SURF COAT, 127(2-3), 2000, pp. 114-119

Authors: Cerisier, M Attenborough, K Celis, JP Van Haesendonck, C
Citation: M. Cerisier et al., Structure and magnetic properties of electrodeposited Co films onto Si(100), APPL SURF S, 166(1-4), 2000, pp. 154-159

Authors: Economou, S De Bonte, M Celis, JP Smith, RW Lugscheider, E
Citation: S. Economou et al., Tribological behaviour at room temperature and at 550 degrees C of TiC-based plasma sprayed coatings in fretting gross slip conditions, WEAR, 244(1-2), 2000, pp. 165-179

Authors: Proost, J Hirato, T Furuhara, T Maex, K Celis, JP
Citation: J. Proost et al., Microtexture and electromigration-induced drift in electroplated damasceneCu, J APPL PHYS, 87(6), 2000, pp. 2792-2802

Authors: Nowak, P Socha, RP Kaisheva, M Fransaer, J Celis, JP Stoinov, Z
Citation: P. Nowak et al., Electrochemical investigation of the codeposition of SiC and SiO2 particles with nickel, J APPL ELEC, 30(4), 2000, pp. 429-437

Authors: Vaes, J Fransaer, J Celis, JP
Citation: J. Vaes et al., The role of metal hydroxides in NiFe deposition, J ELCHEM SO, 147(10), 2000, pp. 3718-3724

Authors: Terzieva, V Fransaer, J Celis, JP
Citation: V. Terzieva et al., Codeposition of hydrophilic and hydrophobic silica with copper from acid copper sulfate baths, J ELCHEM SO, 147(1), 2000, pp. 198-202

Authors: Haseeb, ASMA Celis, JP Roos, JR
Citation: Asma. Haseeb et al., Elastic and plastic properties of electroplated thin films and layered nanocomposites by nanoindentation technique, T I INST ME, 52(6), 1999, pp. 423-426

Authors: Vanhulsel, A Celis, JP Dekempeneer, E Meneve, J Smeets, J Vercammen, K
Citation: A. Vanhulsel et al., Inductively coupled r.f. plasma assisted chemical vapour deposition of diamond-like carbon coatings, DIAM RELAT, 8(7), 1999, pp. 1193-1197