AAAAAA

   
Results: 1-17 |
Results: 17

Authors: Flores, KM Dauskardt, RH
Citation: Km. Flores et Rh. Dauskardt, Mean stress effects on flow localization and failure in a bulk metallic glass, ACT MATER, 49(13), 2001, pp. 2527-2537

Authors: Flores, KM Suh, D Howell, R Asoka-Kumar, P Sterne, PA Dauskardt, RH
Citation: Km. Flores et al., Flow and fracture of bulk metallic glass alloys and their composites, MATER TRANS, 42(4), 2001, pp. 619-622

Authors: Suh, D Dauskardt, RH
Citation: D. Suh et Rh. Dauskardt, Effects of pre-charged hydrogen on the mechanical and thermal behavior of Zr-Ti-Ni-Cu-Be bulk metallic glass alloys, MATER TRANS, 42(4), 2001, pp. 638-641

Authors: Hohlfelder, RJ Maidenberg, DA Dauskardt, RH Wei, YG Hutchinson, JW
Citation: Rj. Hohlfelder et al., Adhesion of benzocyclobutene-passivated silicon in epoxy layered structures, J MATER RES, 16(1), 2001, pp. 243-255

Authors: Lane, MW Snodgrass, JM Dauskardt, RH
Citation: Mw. Lane et al., Environmental effects on interfacial adhesion, MICROEL REL, 41(9-10), 2001, pp. 1615-1624

Authors: Ohashi, KL Yerby, SA Dauskardt, RH
Citation: Kl. Ohashi et al., Effects of an adhesion promoter on the debond resistance of a metal-polymethylmethacrylate interface, J BIOMED MR, 54(3), 2001, pp. 419-427

Authors: Suh, D Dauskardt, RH
Citation: D. Suh et Rh. Dauskardt, Hydrogen effects on the mechanical and fracture behavior of a Zr-Ti-Ni-Cu-Be bulk metallic glass, SCR MATER, 42(3), 2000, pp. 233-240

Authors: Fitzgerald, AM Dauskardt, RH Kenny, TW
Citation: Am. Fitzgerald et al., Fracture toughness and crack growth phenomena of plasma-etched single crystal silicon, SENS ACTU-A, 83(1-3), 2000, pp. 194-199

Authors: Lane, M Dauskardt, RH Vainchtein, A Gao, HJ
Citation: M. Lane et al., Plasticity contributions to interface adhesion in thin-film interconnect structures, J MATER RES, 15(12), 2000, pp. 2758-2769

Authors: Lane, M Dauskardt, RH Krishna, N Hashim, I
Citation: M. Lane et al., Adhesion and reliability of copper interconnects with Ta and TaN barrier layers, J MATER RES, 15(1), 2000, pp. 203-211

Authors: Ohashi, KL Dauskardt, RH
Citation: Kl. Ohashi et Rh. Dauskardt, Effects of fatigue loading and PMMA precoating on the adhesion and subcritical debonding of prosthetic-PMMA interfaces, J BIOMED MR, 51(2), 2000, pp. 172-183

Authors: Bhatnagar, A Hoffman, MJ Dauskardt, RH
Citation: A. Bhatnagar et al., Fracture and subcritical crack-growth behavior of Y-Si-Al-O-N glasses and Si3N4 ceramics, J AM CERAM, 83(3), 2000, pp. 585-596

Authors: Flores, KM Dauskardt, RH
Citation: Km. Flores et Rh. Dauskardt, Enhanced toughness due to stable crack tip damage zones in bulk metallic glass, SCR MATER, 41(9), 1999, pp. 937-943

Authors: Flores, KM Dauskardt, RH
Citation: Km. Flores et Rh. Dauskardt, Local heating associated with crack tip plasticity in Zr-Ti-Ni-Cu-Be bulk amorphous metals, J MATER RES, 14(3), 1999, pp. 638-643

Authors: Yi, KS Cox, BN Dauskardt, RH
Citation: Ks. Yi et al., Fatigue crack-growth behavior of materials in viscous fluid environments, J MECH PHYS, 47(9), 1999, pp. 1843-1871

Authors: Kook, SY Snodgrass, JM Kirtikar, A Dauskardt, RH
Citation: Sy. Kook et al., Adhesion and reliability of polymer/inorganic interfaces, J ELEC PACK, 120(4), 1998, pp. 328-335

Authors: Ohashi, KL Romero, AC McGowan, PD Maloney, WJ Dauskardt, RH
Citation: Kl. Ohashi et al., Adhesion and reliability of interfaces in cemented total joint arthroplasties, J ORTHOP R, 16(6), 1998, pp. 705-714
Risultati: 1-17 |