Authors: AWAJI H TAKAHASHI T YAMAMOTO N HONDA S HIROSAKI N
Citation: H. Awaji et al., ESTIMATION OF THERMAL-SHOCK FRACTURE-TOUGHNESS OF SI3N4, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 106(9), 1998, pp. 877-882

Authors: MUNAKATA F SATOU C HIROSAKI N TANIMURA M AKIMUNE Y INOUE Y
Citation: F. Munakata et al., TEM OBSERVATION OF MICROSTRUCTURE IN SILI CON-NITRIDE CERAMICS CONTAINING Y2O3-ND2O3 ADDITIVE, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 106(4), 1998, pp. 441-443

Authors: MUNAKATA F SATOU C AKIMUNE Y TANIMURA M HIROSAKI N INOUE Y
Citation: F. Munakata et al., EFFECTS OF HYDROTHERMAL TREATMENT ON FIRI NG PROCESS OF SILICON-NITRIDE CONTAINING Y2O3-ND2O3 ADDITIVE, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 106(2), 1998, pp. 208-212

Authors: YASUTOMI Y SAKAIDA Y HIROSAKI N IKUHARA Y
Citation: Y. Yasutomi et al., ANALYSIS OF CRYSTALLOGRAPHIC ORIENTATION OF ELONGATED BETA-SI3N4 PARTICLES IN IN-SITU SI3N4 COMPOSITE BY ELECTRON BACK SCATTERED DIFFRACTION METHOD, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 106(10), 1998, pp. 980-983

Authors: AKIMUNE Y MUNAKATA F HIROSAKI N OKAMOTO Y
Citation: Y. Akimune et al., OPTIMIZATION OF MECHANICAL AND ELECTRICAL -PROPERTIES OF TIN SI3N4 MATERIAL BY AGGLOMERATES-MICROSTRUCTURE-CONTROL (PART 2) - AGGLOMERATE SIZE EFFECT/, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 106(1), 1998, pp. 75-78

Authors: OKAMOTO Y HIROSAKI N ANDO M MUNAKATA F AKIMUNE Y
Citation: Y. Okamoto et al., THERMAL-CONDUCTIVITY OF SELF-REINFORCED S ILICON-NITRIDE CONTAINING LARGE GRAINS ALIGNED BY EXTRUSION PRESSING, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 105(7), 1997, pp. 631-633

Authors: OKAMOTO Y HIROSAKI N AKIMUNE Y MITOMO M
Citation: Y. Okamoto et al., INFLUENCE OF A TO BETA-PHASE TRANSFORMATION ON GRAIN-GROWTH RATE OF SILICON-NITRIDE, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 105(6), 1997, pp. 476-478

Authors: MUNAKATA F TANIMURA M AKIMUNE Y SATOU C INOUE Y HIROSAKI N
Citation: F. Munakata et al., EFFECTS OF HYDROTHERMAL TREATMENT ON FIRI NG PROCESS OF SILICON-NITRIDE CERAMICS, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 105(4), 1997, pp. 347-350

Authors: HIROSAKI N MATSUBARA H
Citation: N. Hirosaki et H. Matsubara, EFFECT OF HEAT-TREATMENT OF SI3N4 ON GRAI N-GROWTH BEHAVIOR AND GRAIN-BOUNDARY STRUCTURE, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 105(3), 1997, pp. 218-222

Authors: AKIMUNE Y MUNAKATA F ANDO M OKAMOTO Y HIROSAKI N
Citation: Y. Akimune et al., OPTIMIZATION OF MECHANICAL AND ELECTRICAL -PROPERTIES OF TIN SI3N4 MATERIAL BY AGGLOMERATES-MICROSTRUCTURE-CONTROL/, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 105(2), 1997, pp. 122-125

Authors: MUNAKATA F SATO C HIROSAKI N TANIMURA M AKIMUNE Y OKAMOTO Y INOUE Y
Citation: F. Munakata et al., ANNEALING EFFECTS FOR STRUCTURAL DEFECTS OF SILICON-NITRIDE CERAMICS, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 105(10), 1997, pp. 858-861

Authors: AKIMUNE Y MUNAKATA F OKAMOTO Y HIROSAKI N
Citation: Y. Akimune et al., TEMPERATURE-DEPENDENCE OF IMPACT DAMAGE I N A SI3N4 DISK BY A SPHERICAL-PARTICLE, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 105(1), 1997, pp. 93-96

Authors: HIROSAKI N ANDO M OKAMOTO Y MUNAKATA F AKIMUNE Y HIRAO K WATARI K BRITO ME TORIYAMA M KANZAKI S
Citation: N. Hirosaki et al., EFFECT OF ALIGNMENT OF LARGE GRAINS ON TH E THERMAL-CONDUCTIVITY OF SELF-REINFORCED BETA-SILICON NITRIDE, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 104(12), 1996, pp. 1171-1173

Authors: HIROSAKI N OKAMOTO Y ANDO M MUNAKATA F AKIMUNE Y
Citation: N. Hirosaki et al., EFFECT OF GRAIN-GROWTH ON THE THERMAL-CON DUCTIVITY OF SILICON-NITRIDE, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 104(1), 1996, pp. 49-53

Authors: HIROSAKI N OKAMOTO Y ANDO M MUNAKATA F AKIMUNE Y
Citation: N. Hirosaki et al., THERMAL-CONDUCTIVITY OF GAS-PRESSURE-SINTERED SILICON-NITRIDE, Journal of the American Ceramic Society, 79(11), 1996, pp. 2878-2882

Authors: HIROSAKI N OKAMOTO Y AKIMUNE Y YAMADA T MITOMO M
Citation: N. Hirosaki et al., SINTERING OF BETA-SI3N4 POWDER MADE BY TH E IMIDE-DECOMPOSITION METHOD, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 103(9), 1995, pp. 977-978

Authors: OGASAWARA T MABUCHI Y HIROSAKI N OKAMOTO Y AKIMUNE Y
Citation: T. Ogasawara et al., FATIGUE BEHAVIOR OF SILICON-NITRIDE CERAM ICS PREPARED FROM BETA-PHASE POWDER, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 103(7), 1995, pp. 709-712

Authors: OKAMOTO Y HIROSAKI N AKIMUNE Y MITOMO M
Citation: Y. Okamoto et al., MECHANICAL-PROPERTIES AND OXIDATION RESIS TANCE OF SILICON-NITRIDE PRODUCED FROM LOW PURITY BETA-POWDER, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 103(7), 1995, pp. 720-723

Authors: HIROSAKI N OKAMOTO Y AKIMUNE Y ISOZAKI K MITOMO M
Citation: N. Hirosaki et al., EFFECT OF PURIFICATION OF BETA-SI3N4 POWD ER ON THE STRENGTH OF SINTERED MATERIALS, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 103(6), 1995, pp. 639-643

Authors: AKIMUNE Y AKIBA T HIROSAKI N DICKINSON JT
Citation: Y. Akimune et al., CHARACTERIZATION OF SI3N4 SURFACE AFTER E XCIMER-LASER RADIATION, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 103(2), 1995, pp. 128-131

Authors: OGASAWARA T HIROSAKI N AKIMUNE Y YASUDA E
Citation: T. Ogasawara et al., FRACTURE-TOUGHNESS AND SUBCRITICAL CRACK- GROWTH OF SMALL CRACK IN SILICON-NITRIDE AT ROOM-TEMPERATURE, Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 103(10), 1995, pp. 1063-1068

Authors: MITOMO M HIROSAKI N HIROTSURU H
Citation: M. Mitomo et al., MICROSTRUCTURAL DESIGN AND CONTROL OF SILICON-NITRIDE CERAMICS, MRS bulletin, 20(2), 1995, pp. 38-41

Authors: AKIBA T AKIMUNE Y HIROSAKI N DICKINSON JT
Citation: T. Akiba et al., PARTICLE-EMISSION FROM SI3N4 SURFACE BY EXCIMER-LASER RADIATION, Journal of materials science letters, 14(12), 1995, pp. 898-900

Authors: KIM YW MITOMO M HIROSAKI N
Citation: Yw. Kim et al., R-CURVE BEHAVIOR AND MICROSTRUCTURE OF SINTERED SILICON-NITRIDE, Journal of Materials Science, 30(20), 1995, pp. 5178-5184

Authors: KIM YV MITOMO M HIROSAKI N
Citation: Yv. Kim et al., R-CURVE BEHAVIOR OF SINTERED SILICON-NITRIDE, Journal of Materials Science, 30(16), 1995, pp. 4043-4048